By controlling the coloring solution
First of all, the colouring solution must be prepared by deionized water. In the case of stannous salt, added H2S04 and stabilizer first, and SnS04 is added after sufficient dissolution to prevent Sn2+ oxidation and hydrolysis. In the case of double salts, SnS04 may be added to the nickel salt solution. liquid of the tank shall be sampled and analyzed at a frequency until the tank is prepared for normal production. According to the analysis results and adding the corresponding agents to stabilize the tank. The control range of the liquid must be stable, and the amount of industrial aluminum profiles must be small and repeated.
The concentration of each component in the tank has a direct effect on the color difference. Generally speaking, the main salt concentration increases, the coloring speeds up, the tone becomes dark; Sulfuric acid is added to the solution to maintain the coloring stability. If the concentration is too high, the tank and parts are easy to adhere to hydroxide. If the concentration is too low, the H+ concentration is too high and slow down the coloring speed.

By controlling anodizing process
Voltage has a great effect on the coloring speed. If the voltage is too low, the peak current of the cathode is very small, which can only be used for blocking layer charging and making up the electric loss. The Faraday current on the deposited metal of industrial aluminum profiles is small, so the color is lighter. As the voltage increases, the current increases and the coloring speed increases, the order of color change of profiles is: slight coloring - champagne - coffee - bronze - brown - black. When the voltage rises to a fixed value, the coloring becomes lighter. This is because, when the voltage is too high and exceeds the oxidation voltage range, the barrier layer is broken down and the colored film falls off, thus the color becomes lighter.