What are the common corrosion types of industrial aluminum? Kaixin Aluminum will introduce them below. Hope it is useful for you.


QC(1)

  • Pitting Corrosion

    Pitting corrosion, also known as spot corrosion, is a very local corrosion form that produces pinprick, dot and hole on metal. Aluminum can be pitted in the atmosphere, fresh water, or in a neutral aqueous solution. Severe pitting can also lead to perforation, but the pitting hole may eventually stop developing and the amount of corrosion remains at a limit. It’s a unique form of anodize reaction, pitting corrosion is an autocatalytic process.


  • Galvanic corrosion
    Galvanic corrosion is also the characteristic corrosion form of aluminum. Aluminum has a very negative potential. When aluminum comes into contact with other metals, it is always at the anode to accelerate its corrosion. Galvanic corrosion is also called bimetallic corrosion. The severity of corrosion is determined by the relative position of two metal potential sequences.


  • Crevice corrosion

    Crevice corrosion is due to the effect of different inflatable batteries, resulting in corrosion acceleration in the gap, but there is no effect outside the gap. Crevice corrosion is not related to the type of alloy, and even very corrosion-resistant alloys will produce crevice corrosion. In recent years, the mechanism of crevice corrosion has been further studied. The acidic environment at the top of crevice is the driving force of corrosion.


  • Intercrystalline corrosion
    Intercrystalline corrosion refers to the  intergranular corrosion of pure aluminum that does not flourish. The reason of intercrystalline corrosion is related to improper heat treatment, Alloying elements or intermetallic compounds precipitate out along the grain boundary. It is the anode that forms the corrosion cell and causes the intercrystalline corrosion acceleration.


  • Filiform corrosion
    Filiform corrosion is a type of subfilm corrosion that develops under the film in the form of a worm-like. This type of film can make paint film or other layers, which generally do not occur under the anodized film.


The above is the type of industrial aluminum corrosion. In fact, the corrosion of industrial aluminum is related to where we place the industrial aluminum. we should pay attention to the storage environment when storing industrial aluminum.